Analysis of the causes of defects in die-cast parts

Author:


1) The design of the die-cast part itself is unreasonable: wall thickness, shape, fillet radius, draft angle, and hole size are inappropriate.
2) Issues with the performance of the die-casting machine: insufficient injection force and clamping force, improper casting pressure and filling speed, mismatch between the size of the casting and the die-casting machine's capacity based on projected area, etc.
3) Problems with the design and manufacturing of die-casting molds: mold alignment, grinding, machining accuracy, the impact of moving parts on casting dimensions, improper layout of cooling water channels.
4) Issues with the die-casting process: improper selection of parting line, design of pouring system, venting grooves, die-casting process parameters, coatings, etc.
5) Problems with alloy materials and melting: inappropriate composition of alloy raw materials, ratio of new to old materials, melting process, etc.
6) Issues with die-casting operations: improper control of material temperature, mold temperature control, process parameter control, spraying, part removal, production cycle, etc.
Any one of the above factors being incorrect or a combination of several factors being incorrect can lead to defects.
Zinc alloy die-cast parts are now used in various product peripherals; various electronic and electrical peripherals are zinc alloy die-cast products. Therefore, there are high requirements for the surface quality of castings and a need for good surface treatment capabilities. The most common defect in zinc alloy cast products is surface bubbling.
Defect characterization: The surface of the die-cast part has small raised bubbles.
① Discovered immediately after die-casting;
② Revealed after polishing or processing;
③ Appears after spraying or electroplating;
④ Appears after being placed for a period of time.
Most surface bubbling in zinc alloys is caused by holes, primarily gas holes and shrinkage holes. Gas holes are often round while shrinkage holes are mostly irregularly shaped.
1. Causes of gas hole formation:
① During the filling and solidification process of molten metal, gas intrusion leads to the formation of holes on the surface or inside the casting;
② Gases released from coatings intrude;
③ Excessive gas content in the alloy liquid precipitates during solidification.
2. Causes of shrinkage hole formation:
① During the solidification process of molten metal, shrinkage in volume or failure to supplement with molten metal at the last solidifying location leads to shrinkage holes;
② Uneven thickness in castings or local overheating causes certain areas to solidify slowly, resulting in depressions on the surface during volume shrinkage.
The presence of gas holes and shrinkage holes can cause issues during surface treatment of die-cast parts. When painting and electroplating are followed by baking, gases inside the holes expand due to heat; or water inside the holes turns into steam, leading to bubbling on the surface of the casting.

Latest Blog

2024-05-23

Precautions for Punching

Punching is a common form of exercise, but there are some precautions to take when performing punches to ensure safety

2024-05-22

Introduction to the application scenarios and functions of punch heads

The punch, as a type of mechanical structural component, plays an important role in industrial production.

2024-05-20

Common issues and solutions for punch heads

During the use of the punch, some common problems may arise that need to be addressed promptly to ensure production

2024-05-19

Analysis of the working principle of a punch head

A punch is a common processing tool widely used in the metalworking field.